| 000 | 00752nab a2200205 4500 | ||
|---|---|---|---|
| 005 | 20260520004235.0 | ||
| 008 | 260224s2011 xxu | ||
| 245 | 0 | 0 | _aPreventing coiled tubing corrosion by hydrochloric acid in hot wells |
| 260 |
_a _b _cmar. 2011 |
||
| 270 | _a01/06/2011 ; 01/06/2011 | ||
| 300 | _a4 p. ; 63-66 | ||
| 520 | _aTranscripción del resumen del autor. Lab testing revealed chemistries capable of maintaining CT integrity while allowing HCl acid concentration sufficient to dissolve calcium carbonate scales | ||
| 581 | _a3 | ||
| 773 | 0 |
_tWorld Oil _g234 |
|
| 942 | _cARTICULO | ||
| 100 | 1 |
_aDanait, Achala _950119 |
|
| 100 | 1 |
_aElliott, Jay _950120 |
|
| 100 | 1 |
_aSabhapondit, Anupom _950121 |
|
| 999 |