245 0 0 _aTesting corrosion rates on steel piping in geothermal district heating
260 _a
_b
_cmayo 2008
270 _a09/08/2010 ; 09/08/2010
300 _a4 p. ; 56-59
520 _aTranscripción del resumen del autor. The St-37 carbon steel piping in a geothermal heating system experienced increasing corrosion leaks. Tests with pipe steel coupons showed that while uniform corrosion rates were low, pitting rates were high. Sulfate-reducing bacteria were the main cause. Changes in fluid velocities and the addition of a bacteriacide were recommended.