| 000 | 00934nab a2200193 4500 | ||
|---|---|---|---|
| 005 | 20260520002915.0 | ||
| 008 | 260224s2009 xxu | ||
| 245 | 0 | 0 | _aResidual stress control to prevent environmental cracking of stainless steels |
| 260 |
_a _b _cdic. 2009 |
||
| 270 | _a02/08/2010 ; 02/08/2010 | ||
| 300 | _a5 p. ; 60-64 | ||
| 520 | _aTranscripción del resumen del autor. Requirements for residual stress control to prevent anodic stress corrosion cracking and hydrogen-induced sulfide stress cracking may significantly affect the delivery/lead time and materials selection for heat exchangers. This study reports microhardness, residual stress, and environmental cracking test results for various stainless steels. | ||
| 581 | _a12 | ||
| 773 | 0 |
_tMaterials Performance _g48 |
|
| 942 | _cARTICULO | ||
| 100 | 1 |
_aMahajanam, Sudhakar P.V. _946111 |
|
| 100 | 1 |
_aMcIntyre, Dale R. _945855 |
|
| 999 |
_c175619 _d175619 |
||