| 000 | 00971nab a2200205 4500 | ||
|---|---|---|---|
| 005 | 20260520002845.0 | ||
| 008 | 260224s2011 xxu | ||
| 245 | 0 | 0 | _aStray current delamination of an organic coating on metallic structures |
| 260 |
_a _b _cene. 2011 |
||
| 270 | _a20/01/2011 ; 20/01/2011 | ||
| 300 | _a5 p. ; 29-33 | ||
| 520 | _aTranscripción del resumen del autor. In this work, the delamination of an organic coating by stray current is investigated. The results indicate that the hydrogen overvoltage potential is exceeded and the primary cathodic reaction is hydrogen evolution. The transport of hydrogen and hydroxyl ions along the coating/metal interface degrades the adhesive strength, forms blisters, and leads to delamination | ||
| 581 | _a1 | ||
| 773 | 0 |
_tMaterials Performance _g50 |
|
| 942 | _cARTICULO | ||
| 100 | 1 |
_aAlin, Cao _944216 |
|
| 100 | 1 |
_aShengtao, Zhang _944217 |
|
| 100 | 1 |
_aQingjun, Zhu _944218 |
|
| 999 |
_c172814 _d172814 |
||