245 0 0 _aDelamination failure in a three-layer coating on a 24-in gas pipeline
_bCase history
260 _a
_b
_cdic. 2010
270 _a10/12/2010 ; 10/12/2010
300 _a6 p. ; 38-43
520 _aTranscripción del resumen del autor. Three-layer pipeline coating systems are commonly used because of the excellent adhesion properties of the fusion-bonded epoxy, water impermeability, and mechanical resistance of the polyolefin. This article describes a disbondament failure that ocurred on a 24-in (610-mm) gas pipeline in Mexico and the steps taken to determine the root cause of the failure