Metal dusting of centrifugally cast superalloys
Publication details: mar. 2011Description: 5 p. ; 62-66 In: Materials Performance 50Summary: Transcripción del resumen del autor. Metal dusting of three centrifugal cast, heat-resistant alloys was investigated in an environment containing 80 vol% carbon monoxide (CO)+20 vol% H2 at 650, 750, and 850°C for 500h. One of the nickel-based alloys experienced localized metal dusting at 650°C and pitting at 750°C. Pitting occurred on another alloy at 650°C. A third nickel alloy was the most resistant to metal dusting, but pitting occurred at 750°C| Current library | Status | Barcode | |
|---|---|---|---|
| Biblioteca Alejandro Angel Bulgheroni | Not for loan | 200052347 |
Transcripción del resumen del autor. Metal dusting of three centrifugal cast, heat-resistant alloys was investigated in an environment containing 80 vol% carbon monoxide (CO)+20 vol% H2 at 650, 750, and 850°C for 500h. One of the nickel-based alloys experienced localized metal dusting at 650°C and pitting at 750°C. Pitting occurred on another alloy at 650°C. A third nickel alloy was the most resistant to metal dusting, but pitting occurred at 750°C
3