Formation and deposition of iron oxides on stainless steel and carbon steel in conditions of secondary circuits of pressurized water reactors

By: Publication details: ene. 2011Description: 10 p. ; 015003 In: Corrosion 67Summary: Transcripción del resumen del autor. An experimental circulating water loop was built to follow the formation, the transport, and the deposition of iron oxides in the feedwater system of the secondary circuit of PWR plants. The test section was made from carbon steel while all other parts of the loop were made from stainless steel. Tests were performedfor 18 days to 101 days in one-phase flow conditions at 150 L/h with a linear velocity between 0.92 m/s and 1.1 m/s at 220°C in an ammonia (NH3) and hydrazine (N2H4) medium. A magnetite (Fe3O4) film appeared on the surface of carbon steel tubes within a few days. Iron oxides were also present on stainless steel segments as goethite (FeOOH) at room temperature and as magnetite at 220°C. The oxide film on carbon steel was heterogeneous and its thickness varied from several µm to 40 µm, while the oxide film on stainless steel did not exceed 2 µm.
Item type: Artículo de Revista
Holdings
Current library Status Barcode
Biblioteca Alejandro Angel Bulgheroni Not for loan 200050726

Transcripción del resumen del autor. An experimental circulating water loop was built to follow the formation, the transport, and the deposition of iron oxides in the feedwater system of the secondary circuit of PWR plants. The test section was made from carbon steel while all other parts of the loop were made from stainless steel. Tests were performedfor 18 days to 101 days in one-phase flow conditions at 150 L/h with a linear velocity between 0.92 m/s and 1.1 m/s at 220°C in an ammonia (NH3) and hydrazine (N2H4) medium. A magnetite (Fe3O4) film appeared on the surface of carbon steel tubes within a few days. Iron oxides were also present on stainless steel segments as goethite (FeOOH) at room temperature and as magnetite at 220°C. The oxide film on carbon steel was heterogeneous and its thickness varied from several µm to 40 µm, while the oxide film on stainless steel did not exceed 2 µm.

1



Instituto Argentino del Petróleo y del Gas
Maipú 639 (C1006ACG) – Buenos Aires – Argentina
Tel: (54 11) 5277 IAPG (4274)
Lu - Vie 11 a 17 hs
Mail: biblio@iapg.org.ar


Copyright © 2026, Instituto Argentino del Petróleo y del Gas, todos los derechos reservados.

Protección de datos personales