Delamination failure in a three-layer coating on a 24-in gas pipeline Case history
Publication details: dic. 2010Description: 6 p. ; 38-43 In: Materials Performance 49Summary: Transcripción del resumen del autor. Three-layer pipeline coating systems are commonly used because of the excellent adhesion properties of the fusion-bonded epoxy, water impermeability, and mechanical resistance of the polyolefin. This article describes a disbondament failure that ocurred on a 24-in (610-mm) gas pipeline in Mexico and the steps taken to determine the root cause of the failure| Current library | Status | Barcode | |
|---|---|---|---|
| Biblioteca Alejandro Angel Bulgheroni | Not for loan | 200050295 |
Transcripción del resumen del autor. Three-layer pipeline coating systems are commonly used because of the excellent adhesion properties of the fusion-bonded epoxy, water impermeability, and mechanical resistance of the polyolefin. This article describes a disbondament failure that ocurred on a 24-in (610-mm) gas pipeline in Mexico and the steps taken to determine the root cause of the failure
12