Synthesis of mesoporous ZnO (m-ZnO) and catalytic performance of the Pd/m-ZnO catalyst for methanol steam reforming
Publication details: mar./abr. 2009Description: 5 p. ; 1342-1346 In: Energy & fuels 23Summary: Resúmen del autor: Mesoporous ZnO (m-ZnO) was successfully synthesized by a supermolecule-templeting approach under hydrothermal conditions, in which triblock co-polymer Pluronic (F-127) was introduced as a template reagent. The corresponding Pd/m-ZnO catalyst was prepared using the deposition-precipitation method, and its catalytic performance was determined in the methanol steam reforming process. Those products were characterized by means of Brunauer-Emmett-Teller surface area (BET), Fourier transform infrared spectroscopy (FTIR), X-ray diffraction analysis (XRD), and H2 temperature-programmed reduction (TPR). In comparison to the Pd/ZnO catalyst, the Pd/m-ZnO catalyst possessed the higher catalytic activity, H2 yield, and CO2 selectivity, which was attributed to the m-ZnO with a larger BET surface area (124.7 m2/g), uniform pore distribution, and stronger interaction with Pd| Current library | Status | Barcode | |
|---|---|---|---|
| Biblioteca Alejandro Angel Bulgheroni | Not for loan | 200045118 |
Resúmen del autor: Mesoporous ZnO (m-ZnO) was successfully synthesized by a supermolecule-templeting approach under hydrothermal conditions, in which triblock co-polymer Pluronic (F-127) was introduced as a template reagent. The corresponding Pd/m-ZnO catalyst was prepared using the deposition-precipitation method, and its catalytic performance was determined in the methanol steam reforming process. Those products were characterized by means of Brunauer-Emmett-Teller surface area (BET), Fourier transform infrared spectroscopy (FTIR), X-ray diffraction analysis (XRD), and H2 temperature-programmed reduction (TPR). In comparison to the Pd/ZnO catalyst, the Pd/m-ZnO catalyst possessed the higher catalytic activity, H2 yield, and CO2 selectivity, which was attributed to the m-ZnO with a larger BET surface area (124.7 m2/g), uniform pore distribution, and stronger interaction with Pd