Characterizing the relaxation of the open-circuit potential during an AC-DC-AC accelerated test

By: Publication details: sep. 2010Description: 11 p. ; 095001 In: Corrosion 66Summary: Transcripción del resumen del autor. The non-conventional accelerated alternating current-direct current-alternating current (AC-DC-AC) testing method for organic coatings induces degradation by promoting cathodic reactions at the metal coating interface and ionic transport in the bulk of the coating. This cyclic method involves a testing step in which the coating properties are determined using electrochemical impedance spectroscopy (EIS), a DC step in which a cathodic potential is applied for a given time period, and a relaxation step where the coating is allowed to relax back to a stable open-circuit potential (EOC) condition. Analysis of the relaxation EOC profile has been reported where characteristic times were attributed to the transport of ions through the coating, dielectric relaxation of the coating, and charge transfer at the metal/coating interface. The AC-DC-AC degradation of a standard United States Army vehicle epoxy primer on a steel substrate is reported here. The influences of applied DC potential and temperature were determined by subjecting the coating to potentials of -2 V and -8 V relative to the stable EOC at temperatures ranging from 25°C to 65°C. The relaxation EOC profiles were analyzed with a mathematical model to yield the characteristic times associated with the processes involved and the consistency of these processes with Arrhenius behavior was determined.
Item type: Artículo de Revista
Holdings
Current library Status Barcode
Biblioteca Alejandro Angel Bulgheroni Not for loan 200048829

Transcripción del resumen del autor. The non-conventional accelerated alternating current-direct current-alternating current (AC-DC-AC) testing method for organic coatings induces degradation by promoting cathodic reactions at the metal coating interface and ionic transport in the bulk of the coating. This cyclic method involves a testing step in which the coating properties are determined using electrochemical impedance spectroscopy (EIS), a DC step in which a cathodic potential is applied for a given time period, and a relaxation step where the coating is allowed to relax back to a stable open-circuit potential (EOC) condition. Analysis of the relaxation EOC profile has been reported where characteristic times were attributed to the transport of ions through the coating, dielectric relaxation of the coating, and charge transfer at the metal/coating interface. The AC-DC-AC degradation of a standard United States Army vehicle epoxy primer on a steel substrate is reported here. The influences of applied DC potential and temperature were determined by subjecting the coating to potentials of -2 V and -8 V relative to the stable EOC at temperatures ranging from 25°C to 65°C. The relaxation EOC profiles were analyzed with a mathematical model to yield the characteristic times associated with the processes involved and the consistency of these processes with Arrhenius behavior was determined.

9



Instituto Argentino del Petróleo y del Gas
Maipú 639 (C1006ACG) – Buenos Aires – Argentina
Tel: (54 11) 5277 IAPG (4274)
Lu - Vie 11 a 17 hs
Mail: biblio@iapg.org.ar


Copyright © 2026, Instituto Argentino del Petróleo y del Gas, todos los derechos reservados.

Protección de datos personales