Corrosion behavior of conventional and spark plasma-sintered Nd-Fe-B permanent magnets in different solutions

By: Publication details: jul. 2009Description: 4 p. ; 501-504 In: Corrosion 65Summary: Transcripción del resumen del autor. Spark plasma sintering (SPS) and conventional sintering techniques were used to fabricate sintered Nd-Fe-B permanent magnets. The corrosion behaviors of both magnets in sodium chloride (NaCl), sodium hydroxide (NaOH), and sulfuric acid (H2SO4) solutions were studied. The weight-loss curves indicate that both magnets exhibit passive behavior in alkaline solution and dissolve actively in acid solution. SEM observations show that the conventional sintered Nd-Fe-B magnets exhibit typical intergranular corrosion. In the SPS magnet, however, intergranular corrosion through the Nd-rich phase is suppressed effectively due to the unique microstructure of the magnets, i.e., the grain size of the Nd2Fe14B main phase is fine and uniform, and the fine Nd-richphase does notform along the grain boundaries of main phase as with conventional magnets, but agglomerates into the triple junctions. As a result, the SPS Nd-Fe-B magnets possess excellent corrosion resistance.
Item type: Artículo de Revista
Holdings
Current library Status Barcode
Biblioteca Alejandro Angel Bulgheroni Not for loan 200047597

Transcripción del resumen del autor. Spark plasma sintering (SPS) and conventional sintering techniques were used to fabricate sintered Nd-Fe-B permanent magnets. The corrosion behaviors of both magnets in sodium chloride (NaCl), sodium hydroxide (NaOH), and sulfuric acid (H2SO4) solutions were studied. The weight-loss curves indicate that both magnets exhibit passive behavior in alkaline solution and dissolve actively in acid solution. SEM observations show that the conventional sintered Nd-Fe-B magnets exhibit typical intergranular corrosion. In the SPS magnet, however, intergranular corrosion through the Nd-rich phase is suppressed effectively due to the unique microstructure of the magnets, i.e., the grain size of the Nd2Fe14B main phase is fine and uniform, and the fine Nd-richphase does notform along the grain boundaries of main phase as with conventional magnets, but agglomerates into the triple junctions. As a result, the SPS Nd-Fe-B magnets possess excellent corrosion resistance.

7



Instituto Argentino del Petróleo y del Gas
Maipú 639 (C1006ACG) – Buenos Aires – Argentina
Tel: (54 11) 5277 IAPG (4274)
Lu - Vie 11 a 17 hs
Mail: biblio@iapg.org.ar


Copyright © 2026, Instituto Argentino del Petróleo y del Gas, todos los derechos reservados.

Protección de datos personales