Stray current delamination of an organic coating on metallic structures

By: Publication details: ene. 2011Description: 5 p. ; 29-33 In: Materials Performance 50Summary: Transcripción del resumen del autor. In this work, the delamination of an organic coating by stray current is investigated. The results indicate that the hydrogen overvoltage potential is exceeded and the primary cathodic reaction is hydrogen evolution. The transport of hydrogen and hydroxyl ions along the coating/metal interface degrades the adhesive strength, forms blisters, and leads to delamination
Item type: Artículo de Revista
Holdings
Current library Status Barcode
Biblioteca Alejandro Angel Bulgheroni Not for loan 200050794

Transcripción del resumen del autor. In this work, the delamination of an organic coating by stray current is investigated. The results indicate that the hydrogen overvoltage potential is exceeded and the primary cathodic reaction is hydrogen evolution. The transport of hydrogen and hydroxyl ions along the coating/metal interface degrades the adhesive strength, forms blisters, and leads to delamination

1



Instituto Argentino del Petróleo y del Gas
Maipú 639 (C1006ACG) – Buenos Aires – Argentina
Tel: (54 11) 5277 IAPG (4274)
Lu - Vie 11 a 17 hs
Mail: biblio@iapg.org.ar


Copyright © 2026, Instituto Argentino del Petróleo y del Gas, todos los derechos reservados.

Protección de datos personales