Flow loop study of NaCI concentration effect on erosion, corrosion, and erosion-corrosion of carbon steel in CO2.saturated systems (Record no. 186961)

MARC details
000 -LEADER
fixed length control field 02187nab a2200241 4500
008 - CÓDIGOS DE INFORMACIÓN DE LONGITUD FIJA - INFORMACIÓN GENERAL
Campo de control de longitud fija 260224s2012 xxu
245 00 - TITULO
Título Flow loop study of NaCI concentration effect on erosion, corrosion, and erosion-corrosion of carbon steel in CO2.saturated systems
260 ## - PUBLICACION, DISTRIBUCION, ETC
Lugar de publicación, distribución, etc.
Nombre de publicador, distribuidor, etc.
Fecha de publicación, distribución, etc. feb. 2012
270 ## - FECHA DE CARGA
Fecha de carga 03/04/2012 ; 03/04/2012
300 ## - DESCRIPCION FISICA
Otra extensión 8 p. ; 026001-1/025001-9
520 ## - RESUMEN, ETC
Resumen Transcripción del resumen del autor: Erosion-corrosion deterioration of carbon steel in carbon dioxide (CO2)-saturated systems with sand is a problem in the oil and gas industry because the combined effects of erosion and corrosion can reduce the protection provided by iron-carbonate scale formation or inhibitors. Oil and gas production can be accompanied by the formation water (typically chloride containing brine). Some effects of chloride concentration on corrosion are not widely known, and this can result in misleading conclusions. The goal of this paper was to contribute to a better understanding of the effects of chloride concentration in CO2 corrosion. Previous studies reported in the literature and experimental and theoretical studies conducted in the present work have shown that increasing the sodium chloride (NaCl) concentration in solution has three important effects on corrosion results. First, standard pH meter readings in high NaCl concentration solutions require corrections. Second, increasing the NaCl concentration decreases the CO2 concentration in solution and therefore contributes to a decrease in the corrosion rate. Third, increasing the NaCl concentration increases the solubility of FeCO3 and therefore reduces the likelihood of forming an iron carbonate scale. High NaCl concentration also decreases the sand erosion rate of the metal slightly by increasing the density and viscosity of the liquid.
581 ## - ESTADO DE COLECCIÓN
Estado de colección 2
773 0# - CORRECCIÓN
Título Corrosion
Partes relacionadas 68
942 ## - DESC. DE MATERIAL
Tipo de item KOHA Artículo de Revista
100 1# - RESPONSABLE PERSONAL
Apellido, Nombre Hassani, Sh.
9 (RLIN) 52290
100 1# - RESPONSABLE PERSONAL
Apellido, Nombre Roberts, K.P.
9 (RLIN) 52291
100 1# - RESPONSABLE PERSONAL
Apellido, Nombre Shirazi, S.A.
9 (RLIN) 16383
100 1# - RESPONSABLE PERSONAL
Apellido, Nombre Shadley, J.R.
9 (RLIN) 52292
100 1# - RESPONSABLE PERSONAL
Apellido, Nombre Rybicki, E.F.
9 (RLIN) 52293
100 1# - RESPONSABLE PERSONAL
Apellido, Nombre Joia, C.
9 (RLIN) 52294
Holdings
Biblioteca propietaria Biblioteca actual Fecha de adquisición Inventario Total de préstamos Inventario Fecha de carga Tipo de item KOHA
Biblioteca Alejandro Angel Bulgheroni Biblioteca Alejandro Angel Bulgheroni 06/03/2026 200059066   200059066 06/03/2026 Artículo de Revista


Instituto Argentino del Petróleo y del Gas
Maipú 639 (C1006ACG) – Buenos Aires – Argentina
Tel: (54 11) 5277 IAPG (4274)
Lu - Vie 11 a 17 hs
Mail: biblio@iapg.org.ar


Copyright © 2026, Instituto Argentino del Petróleo y del Gas, todos los derechos reservados.

Protección de datos personales