Dynamic fracture propagation in hydraulic re-fracturing

By: Publication details: feb. 2010Description: 7 p. ; 266-272 In: Journal of Petroleum Science & Engineering 70Summary: Transcripción del resumen del autor. Re-fracturing is important for stimulating low-permeability reservoirs, for the effective production duration after the initial fracturing is short and needs to be stimulated again. However, the fracture configuration caused by re-fracturing affects the re-stimulated production greatly. Based on fracture mechanics and hydraulic fracturing theory, a model for dynamic path of fracture propagation during re-fracturing is proposed, and computation shows that stress difference and initiation angle contribute to changes in fracture propagation path. The new fracture changes its direction gradually, until to the direction of the maximum horizontal stress. Horizontal stress difference has great obvious influence on fracture dynamic reorientation, the larger the horizontal stress difference is, the shorter the distance of reoriented fracture away from the maximum horizontal stress will be. The predicted paths are in good accordance with those from the surface micro-seismic monitoring and tri-axial large-scale experiments. The model and conclusions are significant to further understanding of re-fracturing process.
Item type: Artículo de Revista
Holdings
Current library Status Barcode
Biblioteca Alejandro Angel Bulgheroni Not for loan 200046020

Transcripción del resumen del autor. Re-fracturing is important for stimulating low-permeability reservoirs, for the effective production duration after the initial fracturing is short and needs to be stimulated again. However, the fracture configuration caused by re-fracturing affects the re-stimulated production greatly. Based on fracture mechanics and hydraulic fracturing theory, a model for dynamic path of fracture propagation during re-fracturing is proposed, and computation shows that stress difference and initiation angle contribute to changes in fracture propagation path. The new fracture changes its direction gradually, until to the direction of the maximum horizontal stress. Horizontal stress difference has great obvious influence on fracture dynamic reorientation, the larger the horizontal stress difference is, the shorter the distance of reoriented fracture away from the maximum horizontal stress will be. The predicted paths are in good accordance with those from the surface micro-seismic monitoring and tri-axial large-scale experiments. The model and conclusions are significant to further understanding of re-fracturing process.

3-4



Instituto Argentino del Petróleo y del Gas
Maipú 639 (C1006ACG) – Buenos Aires – Argentina
Tel: (54 11) 5277 IAPG (4274)
Lu - Vie 11 a 17 hs
Mail: biblio@iapg.org.ar


Copyright © 2026, Instituto Argentino del Petróleo y del Gas, todos los derechos reservados.

Protección de datos personales